#Ironing help?

1 messages · Page 1 of 1 (latest)

crude moat
#

Anyone know how to make super smooth top prints. I clicked ironing and this is what came out. And help on what settings to change?

static vortexBOT
#

Hey @crude moat, thank you for contributing to this forum.
Please provide as much information (images, video, description) as you can. This will increase the chance that someone can help you with your issue.
Use the Close button when your issue is resolved.

crude moat
#

Settings for Original were:
Dynamic Quality
Gyroid infill 20%
PLA 205
Bed 60
Ironing Default

#

Changed settings update:
Standard Quality ✅
Ironing ✅
Monotonic top/bottom order ✅
Monotonic Ironing Order ✅

crude moat
#

Changed settings:
flow increased 10% > 20%
Ironing inset 0.1mm > 0.2mm

crude moat
#

Changed settings:
ironing flow 20% > 25%
Ironing spacing 0.1mm > 0.2mm
Top surface skin layers 0 > 1

nimble totem
#

Higher infill at first

crude moat
nimble totem
#

Yes. If the toplayers sag due too large bridges ironing is having issues

crude moat
#

without layer lines

nimble totem
#

Sure good luck then

crude moat
#

Thanks. The next trial I did 50% infill density just to see. For me sagging doesn’t show or at least what I would think sagging is. I just see lines and some gaps in the lines.

crude moat