#My printer had a massive failure, quality wise, settings and everything was the same now its horrid

1 messages · Page 1 of 1 (latest)

rotund void
#

Supposed to be one piece and it's a Bambu P1S

rotund void
#

Ran a benchy and that came out fine, then put it back on and it came off the baseplate

lofty nightBOT
#
This post has been closed due to inactivity.

This post has been inactive for over 1 hour and so has been closed. To reopen this post simply send another message.

lofty nightBOT
#

Tips for better first layer success

The first layer is quite literally the foundation of a successful print. These are some of the things to keep in mind:

  • Wash your print surface with dish soap and water, refer to ?bedcleaning .
  • Ensure your printing temperatures are appropriate. For PLA, the ideal bed temperature is 55°C-60°C. If the lines appear to come out "gummy" and forms clumps, raising the nozzle temperature may help. Calibrate your nozzle temperature by printing a temperature tower. Refer also to ?platemps .
  • Relevel your bed and ensure your nozzle distance is equally spaced at each corner, refer to ?paperlevel . If your printer is equipped with a bed meshing probe such as a BLTouch or CRTouch, make sure your Z-offset positions the nozzle close enough to the bed, refer to ?z-offset for additional information. If your printer has automatic Z-offset calibration, make sure the nozzle is clean while the calibration runs.
  • You can confirm that your leveling and Z-offset is correct by observing your first layer extrusion by printing a full layer test: Printables, Thingiverse Refer to ?leveling for help with the interpretation of the results.
  • Ensure the nozzle is not colliding with the print. This usually presents itself as loud noises and layer shifting. Some causes may include overextrusion, insufficient cooling, mechanical Z axis issues, or insufficient Z hop
  • For warp-prone materials such as ABS, Nylon, Polypropylene and others an enclosure is recommended, ensure ambient temperatures are high enough (40°C+) and stable. Consider using a specialized bed adhesive.