#Polylight LW - PLA 1.0

11 messages · Page 1 of 1 (latest)

woven sphinx
#

<@&1122587817768398938> When 3D printing Polylight 1.0 LW-PLA with nozzle temp 230°C, bed temp 50°C, 20% fans, 0.5 extrusion multiplier, I get these issues on this particular wing. Can someone give advice please, I really dont know how to fix this. I tried lowering the fan speed as well as changing it higher. I printed at 240°C, etc.

#

benchy looks like this

misty crane
#

That looks wet to me

woven sphinx
#

is there a way to dry it?

vague folio
#

Filament dryer

#

Or something like a food Dehydrator

olive lichen
#

Definiteyl seems wet! You can see the oozing.

#

PLA-LW will anyways string a little bit more and have a bit of a rougher surface though

woven sphinx
#

Okay, but is there really no way to dry it without a filament dryer or food dehydrator

serene sandal
#

Mm doesn't look like moisture to me, LW-PLA is just really stringy. Especially this one because you picked up the active foaming one from 3D Lab Print as opposed to Polymakers PolyLite LW-PLA which is preformed.

woven sphinx
#

Okay that sounds good, but it will get wet sometime and I dont have a Filament dryer or a Food dryer, cant I dry it at all?