#2 Printer Calibration Issues that I can't seem to nail down.

10 messages · Page 1 of 1 (latest)

wet orbit
#

Neptune 2S - PolyLite PLA Pro Black- 6+ Prints at various heat/speed/adhesion settings but all within the specs laid out by Polymaker for that material. All have both issues.

The most recent print used the following specs:
Print Temp 205
Bed Temp 60
Print Speed 50
Fan Speed 100%
Not Retracting at Layer Change
Buildplate Adhesion None

One picture is the material bunching up in one edge/corner near the build plate. All other edges are fine. Any ideas on this one?
The other picture is of the top of the cube and the weird scraped appearance it has, is that normal?

spare valley
#

Top layer indicates too much flow (adjust esteps, slicer flow)

wet orbit
#

im not sure that's a setting I have control over

#

I dont see it in the slicer and my printer has zero settings

#

is it a hardware adjust somewhere?

spare valley
#

What printer is it? Must have missed that part

wet orbit
#

Elegoo Neptune 2S

#

it's my learning printer so I went kinda cheap

spare valley
#

It has V wheels, so make sure those are all tensioned correctly. Also make sure your belts are tensioned (not super tight but not loose)

#

Try to find some community firmware for it if you can