Alright so im trying to increase my quality of prints.
I was printing lithopane and saw i had small blobs. At first i tought wet fillament but then i decided to print a round object using vase mode. And it turned out perfect no blobs at all.
The bloobs seem to be caused when the printer stops at the seems.
How can i go about reducing this. Printer head seems to stop at the seems for like ¼ of a second then restars
Im guessing when the head reaches the seem it stops moving for a small instant but that what causes fillament to ozze out and cause a blob?
Any tips appreciated
Neptune 3 pro
Slicer : cura